Residual Stresses and Distortion in Quenched and Tempered Steels
-
Published:2014
Abstract
In the case of steels, heat treatment plays a fundamental role because no other process step can manipulate the microstructure in order to fulfill such a wide variety of possible in-service conditions. This article addresses heat treatment with regard to hardening and subsequent tempering of steel components in order to optimize tribological properties. It focuses on the heat treatment of tempering and bearing steels and on volume changes that take place due to phase transformations. Plastic deformations that occur due to shrinking and phase transformation are also discussed. The article also describes the generation of thermal, transformation, and hardening...
Sign in
ASM members
Member Sign InM. Schwenk, J. Hoffmeister, V. Schulze, Residual Stresses and Distortion in Quenched and Tempered Steels, Steel Heat Treating Technologies, Vol 4B, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 355–374, https://doi.org/10.31399/asm.hb.v04b.a0005936
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!