Basics of Distortion and Stress Generation during Heat Treatment
-
Published:2014
Abstract
Dimensional and shape changes caused by heat treatment have been the subject of scientific and industrial research for a very long time. This article provides an overview of the complexity of distortion and stress generation during heat treatment of steels. It discusses the measurement and evaluation of dimensional and shape changes with examples. The article describes the mechanisms at work during the generation of stresses and distortion during heat treatment. A hypothetical experiment with increasing application to real life is used to develop a systematization of unavoidable size and shape changes. The article also provides information on the carriers...
Sign in
ASM members
Member Sign InThomas Lübben, Basics of Distortion and Stress Generation during Heat Treatment, Steel Heat Treating Technologies, Vol 4B, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 339–354, https://doi.org/10.31399/asm.hb.v04b.a0005947
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.