Skip Nav Destination
ASM Handbook
Steel Heat Treating Technologies
Edited by
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4B
ISBN electronic:
978-1-62708-166-5
Publication date:
2014
Book Chapter
Heating and Holding Times
-
Published:2014
Page range:
479 - 480
Abstract
Heating time and holding time refer, respectively, to the time required to bring a part to temperature and the time a part is held at the required heat-treatment temperature. This article provides information on heating times and holding times with different types of furnace systems during steel hardening and tempering.
You do not currently have access to this chapter.
Citation
Heating and Holding Times, Steel Heat Treating Technologies, Vol 4B, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 479–480, https://doi.org/10.31399/asm.hb.v04b.a0005992
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Temper Colors for Steels
Heat Treating of Irons and Steels
Iron and Steel
Elementary Materials Science
Water-Hardening Tool Steels
Tool Steels (Fifth Edition)
Air-Hardening, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Acoustical Characterization
Steel Heat Treating Technologies
High-Carbon, High-Chromium, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Oil-Hardening Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Mold Steels
Tool Steels (Fifth Edition)
Heat Treatment of Steel
Metallurgy for the Non-Metallurgist (Second Edition)
The History of Engineering Alloy Steels
The History of Metals in America