This article describes various quenchants, namely, water and inorganic salt solutions, polymers (polyvinyl alcohol, polyalkylene glycol, polyethyl oxazoline, polyvinyl pyrrolidone and sodium polyacrylates), quench oils, and molten salts, which are used for heat treatment of ferrous alloys. It also provides information on the steps for controlling quenching performance for polymer quenchants and oils with an emphasis on measuring quenchant performance, safety measures, and oxidation.

Quenchant agitation can be obtained by circulating quenchant in a quench tank through pumps and impellers. The selection of the agitation method depends on the tank design, type and volume of the quenchant, part design, and the severity of quench required. This article describes flow measurement methods, temperature control, materials handling, and filtration processes during the agitation process. The maintenance of quenching installations is also discussed.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal