Bending of an Aircraft-Wing Slat Track
-
Published:2019
Abstract
During a routine inspection on an aircraft assembly line, an airframe attachment bolt was found to be broken. The bolt was one of 12 that attach the lower outboard longeron to the wing carry-through structure. Failure occurred on the right-hand forward bolt in this longeron splice attachment. The bolt was fabricated from PH13-8Mo stainless steel heat treated to have an ultimate tensile strength of 1517 to 1655 MPa (220 to 240 ksi). A water-soluble coolant was used in drilling the bolt hole where this fastener was inserted. Investigation (visual inspection, 265 SEM images, hardness testing, auger emission spectroscopy and...
Sign in
ASM members
Member Sign InBending of an Aircraft-Wing Slat Track, ASM Failure Analysis Case Histories: Air and Spacecraft, ASM International, 2019, https://doi.org/10.31399/asm.fach.aero.c0092142
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!