Unusual Failure of a Steam Turbine
-
Published:2019
Abstract
Fusing of the switch contacts of a boiler feed pump drive motor led to the failure of a turbine. After rubbing of most of the Ni-Cr steel LP wheels had occurred, due to the admission of water carried over with the steam, a copper-rich alloy from the interstage gland rings melted, penetrated the wheel material, and gave rise to radial and circumferential cracking in four of the LP wheels. It was concluded that when the rotor moved axially and the wheels came into contact with the diaphragms there was a tendency for the former to dish, with the development...
Sign in
ASM members
Member Sign InUnusual Failure of a Steam Turbine, ASM Failure Analysis Case Histories: Power Generating Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.power.c9001484
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!