Thermal Analyses of a Polymer Failure
-
Published:2019
Abstract
Thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC) were used to analyze an automotive polyoxymethylene (POM) sensor housing that was depolymerizing during service. It was found that a combination of heat, oxygen, and sulfuric acid attacked and caused premature failure of the part. POM should not be selected for automotive applications where elevated temperatures and acidic environments can exist. If exposure to acid is suspected, sodium bicarbonate should be applied to neutralize the surrounding environment, followed by copious quantities of water, and repeated until no effervescence is observed.
Sign in
ASM members
Member Sign InRobert P. Kusy, John Q. Whitley, Thermal Analyses of a Polymer Failure, ASM Failure Analysis Case Histories: Automobiles and Trucks, ASM International, 2019, https://doi.org/10.31399/asm.fach.auto.c9001901
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!