Abstract
A suspension bushing separated from the disk on the rear wheel suspension of a racing vehicle while under operation on an express highway, causing the wheel to detach from the car. Visual inspection showed fresh turning grooves at four built-up fillet welds on the torus of the outside of the disk. The welding heat and rapid cooling caused the base material of the disk – already with a martensitic structure – to harden throughout the torus, both of which caused cracking in the inner and outer fillets at the transition from bushing to disk. Visual inspection of the other...
Sign in
ASM members
Member Sign InSuspension Systems, ASM Failure Analysis Case Histories: Automobiles and Trucks, ASM International, 2019
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.