Retrieved Bone Screw Made From Co-Cr-Mo Alloy with Casting Defects
-
Published:2019
Abstract
Threads of a bone screw (Co-Cr-Mo alloy, type ASTM F75) had broken off, and other threads had cracked. 15x sectioning showed porosity, and 155x magnification showed gas holes, segregation, and dissolved oxides. This supports the conclusion that manufacturing defects caused the failure.
You do not currently have access to this chapter.
Citation
Retrieved Bone Screw Made From Co-Cr-Mo Alloy with Casting Defects, ASM Failure Analysis Case Histories: Medical and Biomedical Devices, ASM International, 2019, https://doi.org/10.31399/asm.fach.med.c0089543
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Broken Adjustable Moore Pins Made From Cobalt-Chromium Alloy
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Broken Stem of Femoral Head Component of Total Hip Prosthesis Made From Cast Cobalt-Base Alloy
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Cracked Cast Iron Crankcases
ASM Failure Analysis Case Histories: Processing Errors and Defects
Metal Waves or Laking on Zinc-Based Diecastings
ASM Failure Analysis Case Histories: Processing Errors and Defects
Failure of the Bond Between a Cobalt Alloy Prosthetic Casting and a Sintered Porous Coating
Handbook of Case Histories in Failure Analysis
Gray-Iron Paper-Drier Head Removed from Service
ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
Cracking in a Gray-Iron Cylinder Head Caused by Microporosity
ASM Failure Analysis Case Histories: Automobiles and Trucks
Premature Torquing Failures of Cast A356 Aluminum Actuators
Handbook of Case Histories in Failure Analysis
Investigation on a Damaged Propeller Blade
ASM Failure Analysis Case Histories: Air and Spacecraft
Fatigue Fracture of a Sand-Cast Steel Axle Housing That Originated at a Hot Tear
ASM Failure Analysis Case Histories: Automobiles and Trucks