Plumbing Products
-
Published:2019
Abstract
A section from a stainless steel kitchen sink showed a round red stain on its surface after a short time in storage. Several of these sinks were stacked together and separated by felt pads while in storage, and the mating sink showed a nearly identical stain in the same area, while no stains were noted on any of the other sinks in the stack. The stain was located near one of the pads; however, no discoloration was noted at the pad location. EDS analysis showed the base metal to be austenitic stainless steel, such as type 304. FTIR analysis...
Sign in
ASM members
Member Sign InPlumbing Products, ASM Failure Analysis Case Histories: Household Products and Consumer Goods, ASM International, 2019
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.