This investigation characterizes five surgical stainless steel piercings and one niobium piercing that caused adverse reactions during use, culminating with the removal of the jewelry. Chemical composition shows that none of the materials are in accordance with ISO standards for surgical implant materials. Additionally, none of the stainless steel piercings passed the pitting-resistance criterion of ISO 5832-1, which implies that [%Cr + 3.3(%Mo)] > 26. Under microscopic examination, most of the jewelry revealed the intense presence of linear irregularities on the surface. The lack of resistance to pitting corrosion associated with the poor surface finishing of the stainless steel...
Sign in
ASM members
Member Sign InJewelry, Utensils, and Coins, ASM Failure Analysis Case Histories: Household Products and Consumer Goods, ASM International, 2019
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.