Small-Angle X-Ray and Neutron Scattering
By
D.G. LeGrand
D.G. LeGrand
Polymer Physics and Engineering Branch, Corporate Research and Development, General Electric Company
Search for other works by this author on:
-
Published:1986
Page range:
402 - 406
Abstract
This article presents the experimental and theoretical aspects of small-angle scattering, and discusses specific applications used in the characterization of metals, glasses, polymers, and ceramics. The basic methods of collimating x-rays, the cause of smearing from a line source, desmearing parameters, and the types of scattering curves are illustrated.
You do not currently have access to this chapter.
Citation
D.G. LeGrand, Small-Angle X-Ray and Neutron Scattering, Materials Characterization, Vol 10, Edited By Ruth E. Whan, ASM International, 1986, p 402–406, https://doi.org/10.31399/asm.hb.v10.a0001763
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
Bainitic Structures
Metallography and Microstructures
Massive Transformation Structures
Metallography and Microstructures
Periodic Table of Elements
Fundamentals of Modeling for Metals Processing
Voltammetry
Materials Characterization
Mössbauer Spectroscopy
Materials Characterization
Introduction to Structures in Metals
Metallography and Microstructures
Ion Chromatography
Materials Characterization
Introduction: Atlas of Fractographs
Fractography
Fatigue and Fracture of Ceramics and Polymers
Fatigue and Fracture Understanding the Basics
Gases in Metals
Casting