Neutron Activation Analysis
-
Published:1986
Abstract
Neutron activation analysis (NAA) is a highly sensitive and accurate method of assaying bulk materials for trace levels of many elements. This article provides a detailed account on several types of NAA, namely, nondestructive and radiochemical thermal neutron activation, delayed neutron counting, epithermal and 14-MeV fast neutron activation, and prompt gamma activation analysis. It also includes application examples, explaining where and how each method is used and the types of elements on which they are effective.
Sign in
ASM members
Member Sign InM.E. Bunker, M.M. Minor, S.R. Garcia, Neutron Activation Analysis, Materials Characterization, Vol 10, Edited By Ruth E. Whan, ASM International, 1986, p 233–242, https://doi.org/10.31399/asm.hb.v10.a0001748
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.