Inert Gas Fusion Available to Purchase
-
Published:1986
Abstract
Inert gas fusion is a method of determining the quantitative content of gases in ferrous and nonferrous materials where gases, such as hydrogen, nitrogen, and oxygen, are physically and chemically adsorbed by the materials and later removed and swept by from the fusion area by an inert carrier gas. This article describes the operating principles and sample selection of inert gas fusion. It explains the mechanisms involved in the introduction of fusion gas, separation and detection of fusion gas by thermal-conductive and infrared detection methods. Additionally, the article explains the methods used for analyzing trace amounts of nitrogen, oxygen, and hydrogen in the carrier mediums, providing examples that aid in solving several problems.
R.B. Fricioni, Loren Essig, Inert Gas Fusion, Materials Characterization, Vol 10, Edited By Ruth E. Whan, ASM International, 1986, p 226–232, https://doi.org/10.31399/asm.hb.v10.a0001747
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.