Materials Characterization
Particle-Induced X-Ray Emission
-
Published:1986
Abstract
Particle-induced x-ray emission (PIXE) is one of several quantitative analyses based on characteristic x-rays. This article provides a detailed account on the principles of PIXE, discussing the data-reduction codes used to identify, integrate, and reduce x-ray peaks into elemental concentrations. It provides information on the calibration of PIXE analysis, which is mostly performed using gravimetric standards to avoid serious absorption, refluorescence, or ion energy change corrections. A comparative study on PIXE and x-ray fluorescence is also included. Finally, the article discusses the applications of PIXE in three areas, namely, atmospheric physics and chemistry, external proton milliprobes and historical analysis,...
Sign in
ASM members
Member Sign InThomas A. Cahill, Particle-Induced X-Ray Emission, Materials Characterization, Vol 10, Edited By Ruth E. Whan, ASM International, 1986, p 102–108, https://doi.org/10.31399/asm.hb.v10.a0001734
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!