Fatigue Fracture of a Steel 8 × 19 Elevator Cable
-
Published:2019
Abstract
One of six cables on a passenger elevator was found fractured during a routine inspection. The cable is made of 16-mm steel wire rope designated 8 x 19 G Preformed Extra High Strength Special Traction Elevator Cable with fiber core. Samples of wire from the cable revealed two types of fractures: flat-type fractures were observed in 1.2 and 1 mm diam wires and cup-and-cone fractures were observed in 0.6 mm diam wires. A nick observed in the side of one of the larger wires was found to be rusted. Beach marks radiating inward, indicative of fatigue cracking, were also...
Sign in
ASM members
Member Sign InFatigue Fracture of a Steel 8 × 19 Elevator Cable, ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure, ASM International, 2019, https://doi.org/10.31399/asm.fach.bldgs.c0048039
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!