Skip Nav Destination
View Technical Books >
ASM Failure Analysis Case Histories
ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
ASM International
ISBN electronic:
978-1-62708-230-3
Publication date:
2019
Book Chapter
-
Published:2019
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment, ASM International, 2019
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
A Tin Pest Failure
Handbook of Case Histories in Failure Analysis
Unexpected Corrosion of Type 316L Stainless Steel Neutralization Tanks
Handbook of Case Histories in Failure Analysis
Strategic Materials Availability and Supply
Properties and Selection: Irons, Steels, and High-Performance Alloys
Weld Decay and Stress-Corrosion Cracking in Austenitic Stainless Steel Vessels
ASM Failure Analysis Case Histories: Chemical Processing Equipment
Computational Fluid Dynamics
Materials Selection and Design
Damaged Copper Hot Water Pipe
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
ASTM/ASME Alloy Steels: Atlas of Fractographs
Fractography
Guide to General Information Sources
Thermal Spray Technology
Sizing with Time-of-Flight Diffraction
Nondestructive Evaluation of Materials
Standards and Codes for Nondestructive Testing
Nondestructive Evaluation of Materials