Sand Casting of Aluminum Alloys
-
Published:2018
Abstract
Sand casting processes are typically classified according to the type of binder present in the molding sand mixture. This article discusses common sand casting processes and design considerations related to shape, gating, feeding, and pattern making methods. It describes the composition of sand and binder normally used, and provides information on the aluminum casting alloys produced. The article discusses precision sand casting and sand reclamation, and includes information on health and safety considerations.
Kumar Sadayappan, Abdallah Elsayed, Sand Casting of Aluminum Alloys, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2018, p 193–208, https://doi.org/10.31399/asm.hb.v02a.a0006533