Physical Metallurgy of Aluminum Alloys[1]
-
Published:2018
Abstract
This article provides a thorough review of the physical metallurgy of aluminum alloys and its role in determining the properties and from a design and manufacturing perspective. And its role in include the effects of composition, mechanical working, and/or heat treatment on structure and properties. This article focuses on the effects of alloying and the metallurgical factors on phase constituents, structure, and properties of aluminum alloys. Effects from different combinations of alloying elements are described in terms of relevant alloy phase diagrams. The article addresses the underlying alloying and structural aspects that affect the properties and possible processing routes of aluminum alloys. It provides information on the heat treatment effects on the physical properties of aluminum alloys and the microstructural effects on the fatigue and fracture of aluminum alloys. The important alloying elements and impurities are listed alphabetically as a concise review of major effects.
Junsheng Wang, Physical Metallurgy of Aluminum Alloys, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2018, p 44–79, https://doi.org/10.31399/asm.hb.v02a.a0006503
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.