Book Chapter
Summary of Aluminum Temper Designations
-
Published:2018
Publication history
November 22, 2014
Search within book:
Abstract
This article presents a summary of aluminum temper designations, and applicable aluminum alloys and product forms for temper designations used in the United States (ANSI H35.1), Europe (EN 515), and internationally (ISO 2107).
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Summary of Aluminum Temper Designations, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2018, p 811–814, https://doi.org/10.31399/asm.hb.v02a.a0006531
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Aluminum Alloy Temper Designations and Definitions
Properties and Selection of Aluminum Alloys
Aluminum
Elements of Metallurgy and Engineering Alloys
Aluminum Alloy Nomenclature and Temper Designations
Heat Treating of Nonferrous Alloys
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Laser Beam Machining of Aluminum and Aluminum Alloys
Aluminum Science and Technology
Chemical and Electrolytic Brightening
Aluminum Science and Technology
Aluminum—The Light Metal
The History of Metals in America
Understanding the Corrosion Behavior of Aluminum
Corrosion of Aluminum and Aluminum Alloys
Types of Corrosive Environments
Corrosion of Aluminum and Aluminum Alloys
Etching of Aluminum and Its Alloys
Aluminum Science and Technology