Adhesive bonding is a proven technology in the manufacture of automotive assemblies, helping carmakers achieve weight reduction goals without compromising body stiffness, crash performance, and noise-vibration-handling characteristics. This article discusses the advantages and limitations of adhesive-bonded aluminum joints and the procedures used to produce them. It addresses surface preparation, the addition of interfacial coatings and primers, and the application of thermoplastic and thermosetting resins. The article examines the nature and role of the various layers that constitute the joint and explains how each contributes to performance. It also discusses adhesive selection factors, joint design, and testing procedures.