Sealing of the Anodized Aluminum Coating
-
Published:2018
Abstract
The sealing of the anodized aluminum is a critical process in achieving the durability and extended functionality of anodizing. This article discusses the different methods for sealing the anodic coatings produced by using sulfuric acid, namely, hot deionized water, hot nickel acetate, midtemperature, cold, and dichromate sealing. It reviews the factors that affect seal quality: immersion time, chemistry concentration, temperature, pH, water quality, coating thickness, and contaminants/dye bleeding. The article describes the various tests that are used for determining the quality of the seal, namely, salt spray, modified dye stain, acid dissolution, impedance, copper accelerated acetic acid salt spray, high-alkaline resistance, SO2 fog, and clorox tests.
Pinakin Patel, Tej Patel, Sealing of the Anodized Aluminum Coating, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2018, p 606–610, https://doi.org/10.31399/asm.hb.v02a.a0006499
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!