Etching of Aluminum and Its Alloys
-
Published:2018
Abstract
Etching aluminum can be a pretreatment step for anodizing, chemical conversion coating, metal-to-rubber bonding, and a host of other processes. Chemical etching, using either alkaline or acid solutions, produces a matte finish on aluminum products. This article describes the alkaline etching and acid etching of aluminum. Alkaline etching reduces or eliminates surface scratches, nicks, extrusion die lines, and other imperfections. Acid etching can be done without heavy smut problems, particularly on aluminum die castings. Hydrochloric, hydrofluoric, nitric, phosphoric, chromic, and sulfuric acids are used in acid etching. The article presents a flow chart of the operations used in acid...
Sign in
ASM members
Member Sign InLinda Newman, Etching of Aluminum and Its Alloys, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2018, p 586–589, https://doi.org/10.31399/asm.hb.v02a.a0006489
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.