Aluminum Science and Technology
Semisolid Metal Casting
-
Published:2018
Abstract
Semisolid casting is a near-net shape manufacturing process capable of producing thick- and thin-walled complex-shaped components having excellent mechanical and functional performance. This article begins with a discussion on the history of semisolid processing and the advantages claimed for semisolid casting. It describes the four notable processes used to produce semisolid castings: thixocasting, rheocasting, thixomolding, and wrought processes. Most commercial aluminum semisolid casters use either thixocasting or rheocasting. The article discusses the die design, process conditions, and simulation for semisolid casting. It concludes with a review of several components produced by each of the various semisolid casting processes.
Sign in
ASM members
Member Sign InStephen P. Midson, Semisolid Metal Casting, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2018, p 400–408, https://doi.org/10.31399/asm.hb.v02a.a0006498
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.