Aluminum Science and Technology
Processing of Aluminum Metal-Matrix Composites[1]
Revising author
-
Published:2018
Abstract
In general, metal-matrix composites (MMCs) are classified into three broad categories: continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. This article focuses on stir casting and melt infiltration as the two main methods of MMC solidification processing. It describes the MCC casting methods, such as sand and permanent mold casting, centrifugal casting, compocasting, and high-pressure die casting. The article discusses the MMC infiltration processes in terms of pressure infiltration casting and liquid metal infiltration. It reviews the powder metallurgy processing of aluminum MMCs and deformation processing of discontinuously reinforced aluminum composites. The article concludes with a...
Sign in
ASM members
Member Sign InW.C. Harrigan, Jr., Processing of Aluminum Metal-Matrix Composites, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2018, p 375–386, https://doi.org/10.31399/asm.hb.v02a.a0006488
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!