Fractography
ASTM/ASME Alloy Steels: Atlas of Fractographs
-
Published:1987
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of ASTM/ASME alloy steels and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the solidification cracking, creep failure, brittle fracture, fracture by overpressurization, inclusion effect, fatigue crack propagation, ductile fatigue striation, secondary cracking, intergranular fracture, and elevated-temperature fracture of alloy steels used in pressure vessels, steam boiler superheater tubes, and box-girder bridges.
Sign in
ASM members
Member Sign InASTM/ASME Alloy Steels: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 291–296, https://doi.org/10.31399/asm.hb.v12.a0000609
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.