Maraging Steels: Atlas of Fractographs
-
Published:1987
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of maraging steels and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the tensile-test fracture, low-cycle fatigue fracture, fibrous fracture, crack-initiation zone, microvoid coalescence, fatigue-crack surface, hydrogen embrittlement, and fatigue striations of these steels.
You do not currently have access to this chapter.
Citation
Maraging Steels: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 383–387, https://doi.org/10.31399/asm.hb.v12.a0000614
Download citation file:
Related Book Content
Cast Aluminum Alloys: Atlas of Fractographs
Fractography
Cobalt Alloys: Atlas of Fractographs
Fractography
Martensitic Stainless Steels: Atlas of Fractographs
Fractography
Gray Irons: Atlas of Fractographs
Fractography
Copper Alloys: Atlas of Fractographs
Fractography
Maraging Steels
Alloying Understanding the Basics
Low-Carbon Steels: Atlas of Fractographs
Fractography
Medium-Carbon Steels: Atlas of Fractographs
Fractography
High-Carbon Steels: Atlas of Fractographs
Fractography