Ductile Irons: Atlas of Fractographs
-
Published:1987
Page range:
227 - 237
Abstract
This article is an atlas of fractographs that covers pearlitic and ferritic ductile irons. The fractographs display the following: brittle cleavage fracture; fatigue crack propagation; fatigue and monotonic fracture surfaces; fracture modes in slow monotonic loading and impact loading; and microcrack initiation and propagation.
You do not currently have access to this chapter.
Citation
Ductile Irons: Atlas of Fractographs, Fractography, Vol 12, By ASM Handbook Committee, ASM International, 1987, p 227–237, https://doi.org/10.31399/asm.hb.v12.a0000603
Download citation file:
Related Book Content
Probabilistic Damage Tolerance Analysis of Gas Turbine Rotors
ASM Failure Analysis Case Histories: Air and Spacecraft
Failure of a Rubber Office-Chair Roller
ASM Failure Analysis Case Histories: Household Products and Consumer Goods
Modes of Fracture
Fractography
Titanium Alloys: Atlas of Fractographs
Fractography
Fracture Analysis
Cast Iron Science and Technology
Wrought Aluminum Alloys: Atlas of Fractographs
Fractography
Fatigue Failure of Six Cap Screws From a Hydraulic Coupling
Handbook of Case Histories in Failure Analysis
Fatigue Fracture of Modified 1035 Steel Cap Screws
ASM Failure Analysis Case Histories: Automobiles and Trucks
Another Turbogenerator Failure
ASM Failure Analysis Case Histories: Power Generating Equipment
Transmission Electron Microscopy
Fractography