Ceramics: Atlas of Fractographs
-
Published:1987
Page range:
471
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of two types of ceramics, namely, boron- and carbon-doped silicon carbide.
You do not currently have access to this chapter.
Citation
Ceramics: Atlas of Fractographs, Fractography, Vol 12, By ASM Handbook Committee, ASM International, 1987, p 471, https://doi.org/10.31399/asm.hb.v12.a0000627
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Ceramics
Machining
Friction and Wear of Ceramics
Friction, Lubrication, and Wear Technology
Concrete and Asphalt: Atlas of Fractographs
Fractography
Nickel Alloys: Atlas of Fractographs
Fractography
Resin-Matrix Composites: Atlas of Fractographs
Fractography
Cobalt Alloys: Atlas of Fractographs
Fractography
Metal-Matrix Composites: Atlas of Fractographs
Fractography
Martensitic Stainless Steels: Atlas of Fractographs
Fractography
Electronic Materials: Atlas of Fractographs
Fractography
Maraging Steels: Atlas of Fractographs
Fractography