Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of a type of resin-matrix composites, carbon-epoxy composites. The fractographs illustrate the fracture modes found in composite prepregs, composite panels, solid rocket motor nozzles, and tension, flexural, compressive, and shear loadings.
You do not currently have access to this chapter.
Citation
Resin-Matrix Composites: Atlas of Fractographs, Fractography, Vol 12, By ASM Handbook Committee, ASM International, 1987, p 474–478, https://doi.org/10.31399/asm.hb.v12.a0000629
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Effects of Composition, Processing, and Structure on Properties of Composites
Materials Selection and Design
Concrete and Asphalt: Atlas of Fractographs
Fractography
Nickel Alloys: Atlas of Fractographs
Fractography
Ceramics: Atlas of Fractographs
Fractography
Cobalt Alloys: Atlas of Fractographs
Fractography
Metal-Matrix Composites: Atlas of Fractographs
Fractography
Martensitic Stainless Steels: Atlas of Fractographs
Fractography
Electronic Materials: Atlas of Fractographs
Fractography
Maraging Steels: Atlas of Fractographs
Fractography
Introduction to Environmental Performance of Nonmetallic Materials
Corrosion: Materials