Precipitation-Hardening Stainless Steels: Atlas of Fractographs
-
Published:1987
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of precipitation-hardening stainless steels and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the cup-and-cone tension-overload fracture, low-cycle and high-cycle fatigue fracture, fracture surface, brittle intergranular fracture, hydrogen embrittlement, and intergranular stress-corrosion cracking of stainless steel components of these steels. The components include high-pressure compressor parts, springs, deflector yokes of aircraft main landing gears, and aircraft engine mount beams.
Precipitation-Hardening Stainless Steels: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 370–374, https://doi.org/10.31399/asm.hb.v12.a0000612
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.