Malleable Irons/White Irons: Atlas of Fractographs
-
Published:1987
Page range:
238 - 239
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of pearlitic malleable and ferritic malleable white irons, and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the fracture sequence, localized plastic deformation, and microcrack initiation and propagation of these irons.
You do not currently have access to this chapter.
Citation
Malleable Irons/White Irons: Atlas of Fractographs, Fractography, Vol 12, By ASM Handbook Committee, ASM International, 1987, p 238–239, https://doi.org/10.31399/asm.hb.v12.a0000604
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Fatigue Testing and Behavior
Characterization and Failure Analysis of Plastics
Mechanisms of Stress-Corrosion Cracking
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Stress-Corrosion Cracking
Corrosion in the Petrochemical Industry (Second Edition)
Stress-Corrosion Cracking
Corrosion: Fundamentals, Testing, and Protection
Fatigue Failure
Characterization and Failure Analysis of Plastics
Fracture and Fractography
Characterization and Failure Analysis of Plastics
Failure of a First-Stage Compressor Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Fatigue Strength of Metals
Mechanics and Mechanisms of Fracture An Introduction
Fracture of Plastics
Characterization and Failure Analysis of Plastics
Cracking in an Aircraft Nose Landing Gear Strut
Handbook of Case Histories in Failure Analysis