Brazing of Conventional Titanium Alloys[1]
-
Published:1993
Abstract
This article discusses the effects of brazing temperature and thermal treatment on structure and mechanical behavior of different classes of titanium base metals such as commercially pure (CP) titanium, alpha or near-alpha alloys, alpha-beta alloys, and beta alloys. The classification, properties, and potential heat treatment of titanium base alloys are presented in tables. The article provides information on brazed joints of titanium with carbon steels, as well as ceramics and graphite. It discusses the risks involved in titanium brazing, including erosion of base metal, brittle intermetallics, and low ductility. The article reviews induction and torch brazing, infrared brazing, diffusion...
Sign in
ASM members
Member Sign InAlexander E. Shapiro, Brazing of Conventional Titanium Alloys, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1–25, https://doi.org/10.31399/asm.hb.v06.a0009239
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!