Abstract
This article discusses the effects of brazing temperature and thermal treatment on structure and mechanical behavior of different classes of titanium base metals such as commercially pure (CP) titanium, alpha or near-alpha alloys, alpha-beta alloys, and beta alloys. The classification, properties, and potential heat treatment of titanium base alloys are presented in tables. The article provides information on brazed joints of titanium with carbon steels, as well as ceramics and graphite. It discusses the risks involved in titanium brazing, including erosion of base metal, brittle intermetallics, and low ductility. The article reviews induction and torch brazing, infrared brazing, diffusion brazing, and brazing by heating with ion bombardment. It concludes by describing the design criteria and limitations of brazing.
Alexander E. Shapiro, Brazing of Conventional Titanium Alloys, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1–25, https://doi.org/10.31399/asm.hb.v06.a0009239
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.