Welding of Titanium Alloys
Revising author
Consultant
-
Published:1993
Abstract
Commercially pure titanium and most titanium alloys can be welded by procedures and equipment used in welding austenitic stainless steel and aluminum. This article describes weldability of unalloyed titanium and all alpha titanium alloys. It reviews the selection of fusion-welding processes that are used for joining titanium and titanium alloys. The processes include gas-tungsten arc welding (GTAW), gas-metal arc welding (GMAW), plasma arc welding (PAW), electron-beam welding (EBW), laser-beam welding (LBW), friction welding (FRW), and resistance welding (RW). The article discusses the role of filler metals and shielding gases in welding titanium and titanium alloys. It describes the equipment used for gas-tungsten arc welding and concludes with information on repair welds.
R. Terrence Webster, Welding of Titanium Alloys, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 783–786, https://doi.org/10.31399/asm.hb.v06.a0001440
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.