Cracking Phenomena Associated With Welding
-
Published:1993
Abstract
This article discusses four types of defects in materials that have been fusion welded and that have been the focus of much attention because of the magnitude of their impact on product quality. These include hot cracks, heat-affected zone (HAZ) microfissures, cold cracks, and lamellar tearing. These defects, all of which manifest themselves as cracks, are characteristic of phenomena that occur at certain temperature intervals specific to a given alloy. The article presents selected alloy 625 compositions used in weldability study.
Sign in
ASM members
Member Sign InMichael J. Cieslak, Cracking Phenomena Associated With Welding, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 88–96, https://doi.org/10.31399/asm.hb.v06.a0001342
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!