Abstract
Welding codes and standards usually require the qualification of welding procedures prior to being used in production. This is to ensure that welds will meet the minimum quality and mechanical property requirements for the application. This article provides an overview of the welding procedure qualification guidelines and test methods. It also reviews the codes, standards, and specifications that govern the design and fabrication of welded structures for the procedure qualification details that are appropriate for a given application.
Sign in
ASM members
Member Sign InHarvey R. Castner, Weld Procedure Qualification, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1089–1093, https://doi.org/10.31399/asm.hb.v06.a0001474
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.