Abstract
This article describes the applications, methods, and limitations of five principal nondestructive test methods, namely, penetrant testing, magnetic-particle testing, eddy current testing, radiographic testing, and ultrasonic testing. The article also provides guidance for the method selection for respective applications.
Topics
Weld corrosion,
Brazing,
Soldering,
Welding,
Brazeability,
Process modeling and simulation,
Joinability,
Solderability,
Weldability,
Mechanical and machine components,
Nondestructive testing,
Eddy current inspection,
Magnetic particle inspection,
Industrial radiography,
Liquid penetrant inspection,
Ultrasonic inspection,
Inspection
You do not currently have access to this chapter.
Citation
G.R. Edwards, Inspection of Welded Joints, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1081–1088, https://doi.org/10.31399/asm.hb.v06.a0001473
Download citation file:
Related Book Content
Nondestructive Evaluation Applications for Failure Analysis
Failure Analysis and Prevention (2021 Edition)
Nondestructive Testing
Composites
Torsional Fatigue Failure of Crane Shaft
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Burst Copper Evaporator Tubes in an Absorption Air-Conditioning Unit
ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure
Stud Arc Welding
Welding Fundamentals and Processes
Design Considerations for Electron Beam Welding
Welding Fundamentals and Processes
Damage Assessment in a Kevlar/Polyester Composite Component
ASM Failure Analysis Case Histories: Air and Spacecraft
Fracture of the Low Carbon Steel Tail Shaft on a Tanker Ship
ASM Failure Analysis Case Histories: Offshore, Shipbuilding, and Marine Equipment
Use of Ultrasonic Inspection to Detect Creep Rupture in Stainless Steel Headers of an Ammonia-Plant Reformer Furnace
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Failure of a Large Gas Cylinder Due to Internal Laminar Defects
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms