Coextrusion Welding
-
Published:1993
Abstract
Coextrusion welding (CEW) is a solid-state process that produces a weld by heating two or more workpieces to the welding temperature and forcing them through an extrusion die. This article describes cold and hot CEW for common metals such as low-carbon steel, aluminum, aluminum alloys, copper, and copper alloys. Additional applicable materials include nickel, nickel-base alloys, zirconium, titanium, tantalum, and niobium.
Coextrusion Welding, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 311, https://doi.org/10.31399/asm.hb.v06.a0001379