Cold pressure welding can be accomplished by deforming in a lap or butt configuration, drawing, extrusion, and rolling. This article provides a discussion on cold pressure lap welding, cold pressure butt welding and cold pressure welding in drawing process with illustrations. It provides information on the combinations of metals that can be successfully cold welded.