Plasma-MIG Welding[1] Available to Purchase
-
Published:1993
Abstract
Plasma-metal inert gas (MIG) welding can be defined as a combination of plasma arc welding (PAW) and gas-metal arc welding (GMAW) within a single torch, where a filler wire is fed through the plasma nozzle orifice. This article describes the principles of operation and operating modes of plasma-MIG welding. It discusses the advantages and disadvantages of the plasma-MIG process. The article describes the components, including power sources and welding torches, of equipment used for the plasma-MIG process. It provides information on inspection and weld quality control and troubleshooting techniques. The article concludes with a discussion on the applications of the plasma-MIG process.
Ian D. Harris, Plasma-MIG Welding, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 223–225, https://doi.org/10.31399/asm.hb.v06.a0001362
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.