Welding, Brazing, and Soldering
Brazing of Copper, Copper Alloys, and Precious Metals
-
Published:1993
Abstract
Copper, copper alloys, and precious metals are probably the most easily brazed metals because of their resistance to oxidation at high temperatures. This article provides a brief discussion on the metallurgy of copper, copper alloys, and precious metals and discusses the filler metals, brazing fluxes, joint clearance and design, and different brazing processes used in brazing of copper, copper alloys, and precious metals.
Sign in
ASM members
Member Sign InRoy E. Beal, Rodger E. Cook, Brazing of Copper, Copper Alloys, and Precious Metals, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 931–936, https://doi.org/10.31399/asm.hb.v06.a0001454
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.