Brazing of Heat-Resistant Alloys, Low-Alloy Steels, and Tool Steels
Revising author
-
Published:1993
Abstract
This article focuses primarily on the various steps involved in the brazing of heat-resistant alloys (nickel- and cobalt-base alloys). The major steps include the selection of brazing filler metals, surface cleaning and preparation, brazing processes and their corresponding atmospheres, and fixturing. The article also provides an overview of the brazing of blow-alloy steels and tool steels and oxide dispersion-strengthened alloys.
Darrell Manente, Brazing of Heat-Resistant Alloys, Low-Alloy Steels, and Tool Steels, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 924–930, https://doi.org/10.31399/asm.hb.v06.a0001453