Low-Temperature Solid-State Welding Available to Purchase
-
Published:1993
Abstract
This article describes low-temperature solid-state welding processes in relation to the interlayer fabrication method, welding method, and welding parameters. The interlayer fabrication method is used to produce vacuum coated interlayers, electrodeposited interlayers, and foil interlayers. The article discusses welding methods, including uniaxial compression and hot isostatic pressing. The article provides information on the effect of base-metal surface finish on the tensile strength of joints solid-state welded using silver interlayers in tabular form and addresses the surface cleaning steps of base-metals.
R.S. Rosen, Low-Temperature Solid-State Welding, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 300–302, https://doi.org/10.31399/asm.hb.v06.a0001375
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.