Abstract
This article describes the principles of operation, operating techniques, equipment selection, and important process variables of air-carbon arc cutting. It also provides information on the safety practices to be followed during the air-carbon arc cutting process.
You do not currently have access to this chapter.
Citation
Robert L. Strohl, Air-Carbon Arc Cutting, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1172–1177, https://doi.org/10.31399/asm.hb.v06.a0001485
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
Plasma Arc Cutting
Welding, Brazing, and Soldering
Oxyfuel Gas Cutting
Welding, Brazing, and Soldering