Carbon arc welding (CAW) utilizes a nonconsumable electrode, made of carbon or graphite, to establish an arc between itself and either a workpiece or another carbon electrode. This article describes the operation modes of the CAW process: single-electrode operation and twin-electrode operation. It presents a schematic representation of typical arrangements for single-electrode and twin-electrode carbon arc welding. Recommended current ranges for carbon and graphite electrodes are listed in a table. The article concludes with information on the applications of the CAW process.
Lance Soisson, Carbon Arc Welding, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 200–201, https://doi.org/10.31399/asm.hb.v06.a0001358
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.