Welding, Brazing, and Soldering
Abstract
This article discusses factors involved in selecting welding processes and consumables and establishing procedures and practices for the arc welding of low-alloy steels. It provides information on welding consumables in terms of filler metals and fluxes and shielding gases. The article describes the various categories of low-alloy steels, such as high-strength low-alloy (HSLA) structural steels, high-strength low-alloy quenched and tempered(HSLA Q&T) structural steels, low-alloy steels for pressure vessels and piping, medium-carbon heat-treatable (quenched and tempered) low-alloy (HTLA) steels, ultrahigh-strength low-alloy steels, and low-alloy tool and die steels. It concludes with a discussion on repair practices for tools and dies....
Sign in
ASM members
Member Sign InF.J. Winsor, Welding of Low-Alloy Steels, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 662–676, https://doi.org/10.31399/asm.hb.v06.a0001433
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.