Brazing With Clad Brazing Materials
-
Published:1993
Abstract
This article focuses on clad brazing material, which is defined as any base material or alloy that is clad with an appropriate lower-melting-point brazing filler metal. It provides information on typical clad brazing strip products in a tabular form and lists the advantages of using clad brazing materials. The article compares the steps in using brazing preforms to fabricate a brazed assembly with the steps involved in using clad brazing materials. It concludes with a discussion on design and manufacturing considerations, during brazing with clad brazing materials.
Sign in
ASM members
Member Sign InSunil Jha, Michael Karavolis, Kevin Dunn, James Forster, Brazing With Clad Brazing Materials, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 347–348, https://doi.org/10.31399/asm.hb.v06.a0001392
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.