This article focuses on clad brazing material, which is defined as any base material or alloy that is clad with an appropriate lower-melting-point brazing filler metal. It provides information on typical clad brazing strip products in a tabular form and lists the advantages of using clad brazing materials. The article compares the steps in using brazing preforms to fabricate a brazed assembly with the steps involved in using clad brazing materials. It concludes with a discussion on design and manufacturing considerations, during brazing with clad brazing materials.