Numerical Aspects of Modeling Welds Available to Purchase
-
Published:1993
Abstract
This article focuses on the various assumptions involved in the numerical modeling of welds, including the geometry of the welded structure and the weld joint, thermal stress, strain, residual stress, and the microstructure in the heat-affected and fusion zones.
John Goldak, Moashi Gu, Lennart Karlsson, Numerical Aspects of Modeling Welds, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1131–1140, https://doi.org/10.31399/asm.hb.v06.a0001480